Natural Weathering of Wood Heat-Treated at 220℃

When wood is exposed to natural weathering and UV radiation discoloration progresses. The color variation of heat-treated wood was investigated. Four domestic species were selected and heat-treated at 220℃ and naturally weathered for 42 days. Their colors were measured with a portable colorimeter. The color variations were different between species. The Korean red pine specimens were highly discolored by the natural weathering even though they were heat-treated. In contrast to Korean red pine, Korean pine is less discolored. The maximum color difference of larch was lower than Korean red pine. All specimens of birch exceeded the color difference criterion of 15 after 25 hours with the maximum of 28.

INTRODUCTION

MATERIAL AND METHODS

RESULTS AND DISCUSSION

SUMMARY

REFERENCES